Average - temperature catalyst “OHK-02”

Average - temperature catalyst “OHK-02”

THE CATALYST OF MEDIUM TEMPERATURE

OF CARBON OXIDE CONVERSION (II) «OXK-02»

KSt 6.3-105:2009 (CN of FEA code 381 590 9000)

The catalysts «OXK-02» and «OXK-02E» are designed for steam reforming of carbonic oxide process under pressure up to 5 MPa and under the temperatures (320÷350). The production of pilot batch of catalyst «OXK-02» was conducted in 2001 for commercial reactor loading with the purpose of experimental-industrial tests.

Specifications

OXK-02

OXK-02E

Physical configuration

tablets of cylindrical form of brown color

extrusions of cylindrical form of brown color

Size of tablets, mm

- diameter

- height

6,0±0,2

6,5±0,5

6,0±0,2

5,0±20,0

Bulk density, kg/dm3

1,4±0,2

1,3±0,3

Mechanical strength-breaking force in crushing along generatrix, МPа, no less than

- average

- minimum

2,5

1,2

2,5

1,5

Mass fraction of wastage while transfixion under the in (900±10)° С, %, no more than

15

15

Mass fraction of iron on conversion to iron oxide (III) (Fe2O3), %,

85

85

Mass fraction of chrome on conversion to (III) (Cr2O3), %, no less than

6,2÷7,0

6,2÷7,0

Mass fraction of copper on conversion to copper oxide (II) (CuO), %

3,0÷5,0

3,0÷5,0

Mass fraction of sulfur on conversion to elementary S, %, no more than

0,05

0,05

Mass fraction of natrium on conversion to sodium oxide (Na2O), %, no more than

0,15

0,15

Activity at reaction rate constant under Т=350оС, sm3/gs, no less than

1,2

1,2

Safety requirements: in accordance with regulations.

Packaging: in clean, tightly closed container.

Transportation: by all modes of transport, except air and sea transportation.


 